Sign In | Join Free | My portofva.com |
|
Brand Name : BaoYang
Model Number : ASTM A213 T11 T22 T91 T12 T92 T5 T9
Certification : CE & ISO
Place of Origin : cangzhou
MOQ : 1
Price : Negotiable
Payment Terms : L/C, D/A, D/P, T/T, Western Union
Delivery Time : 7~30 working days
Packaging Details : Standard Export Packing
Name : High Pressure Boiler Steel Pipe
Process : Hot Rolled Cold Rolled Cold Drawn
Standards : ASTM A213 T11 T22 T91 T12 T92 T5 T9
Material : Carbon Steel
Wall Thickness : 1-20mm (0.04 Inch - 0.78 Inch)
Outer Diameter : 6-2500mm
Processing Service : Bending, Punching, Cutting
Usage : Pipeline Transport, Oil/Gas Drilling, Machinery Industry
Parameter | Description |
---|---|
Grades | ASTM A213 T11, T22, T91, T12, T92, T5, T9 |
Material | Alloy Steel (Seamless) |
Standard | ASTM A213 |
Size Range | Various diameters and wall thicknesses as per ASTM A213 |
Length | Standard lengths, customizable upon request |
Ends | Plain ends, beveled ends, threaded, or socket-weld ends |
Surface Treatment | As-rolled, annealed, or normalized |
Property | Requirement by Grade |
---|---|
Tensile Strength | Varies by grade, typically from ≥415 MPa to ≥620 MPa (60,000 to 90,000 psi) |
Yield Strength | Varies by grade, typically from ≥205 MPa to ≥415 MPa (30,000 to 60,000 psi) |
Elongation | Typically ≥20% in 50 mm (2 in) or 4D, whichever is greater |
Hardness | Varies depending on heat treatment and specific grade |
Element | Typical Range (%) by Grade (Examples) |
---|---|
Carbon | Varies, e.g., T11: 0.04-0.10 |
Chromium | Some grades contain chromium, e.g., T91: 8.00-9.50 |
Manganese | Typically 0.35-0.60 |
Phosphorus | ≤ 0.025 (common across grades) |
Sulfur | ≤ 0.025 (common across grades) |
Silicon | Typically ≤ 0.50 |
![]() |
Alloy High Pressure Boiler Steel Pipe ASTM A213 T11 T22 T91 T12 T92 T5 T9 Images |